Kokskaidu granulu īpašības
ENPlus A1
ENPlus A2
Mytrums
| ENPlus A1 | ≤ 10,0% |
| Actual | 4.7% |
Palnu saturs
| ENPlus A1 | ≤ 0,7% |
| Actual | 0,44% |
Syltumspieja
| ENPlus A1 | ≥ 16,5 MJ/kg |
| Actual | 17,9 MJ/kg |
Tylpuma bleivums
| ENPlus A1 | 600 ≤ BD ≤ 750 |
| Actual | 690 kg/m3 |
Diametrs
| ENPlus A1 | 6 ± 1 mm |
| Actual | 6 mm |
Mehaniskuo iztureiba
| ENPlus A1 | ≥ 98% |
| Actual | 98,3% |
Smolkumi (<3,15)
| ENPlus A1 | ≤ 1% |
| Actual | 0,1% |
Sluopeklis
| ENPlus A1 | ≤ 0,3% |
| Actual | 0,13% |
Palnu deformacejis temperatura
| ENPlus A1 | ≥ 1200℃ |
| Actual | 1330℃ |
Mytrums
| ENPlus A2 | ≤ 10,0% |
| Actual | 5,5% |
Palnu saturs
| ENPlus A2 | ≤1,2 % |
| Actual | 0,86% |
Syltumspieja
| ENPlus A2 | ≥ 16,5 MJ/kg |
| Actual | 17,7 MJ/kg |
Tylpuma bleivums
| ENPlus A2 | 600 ≤ BD ≤ 750 |
| Actual | 670 kg/m3 |
Diametrs
| ENPlus A2 | 6 ± 1 mm |
| Actual | 6,1mm |
Mehaniskuo iztureiba
| ENPlus A2 | ≥ 97,5% |
| Actual | 97,7% |
Smolkumi (<3,15)
| ENPlus A2 | ≤ 1% |
| Actual | 0,1% |
Sluopeklis
| ENPlus A2 | ≤0,5% |
| Actual | 0,18% |
Palnu deformacejis temperatura
| ENPlus A2 | ≥ 1110℃ |
| Actual | 1390℃ |